Specifications and Other Information of Our Electrolyte for NCM with high nickel
Detailed Specification
Grade 1
Electrolyte grade
WI398
Warranty period
6 months(Unopened)
Cathode material
NCM
Solvent composition
EC/DEC/EMC/PC
Anode material
Composite graphite, Artificial graphite
Moisture content
≤15ppm
Cycle performance
After 2000 cycles the capacity retention remains 80% at IC/IC
Acidity content
≤50ppm
Applicable battery
Soft package, Aluminum shell
Density
>1,20g/mL
Low temperature performance
Under-20℃ and for 16 hours, Capacitance play is more than 70% at 0.2C
Conductivity
6.5-8.5ms/cm
High temperature performance
Under 60℃ under for 7 days with full charge, the expansion rate is less than 5%
Chroma
≤50Hazen
Grade 2
Electrolyte grade
WI65
Warranty period
6 months(Unopened)
Cathode material
NCM
Solvent composition
EC/DEC/EMC/PC
Anode material
Composite graphite, Artificial graphite
Moisture content
≤15ppm
Cycle performance
After 2000 cycles the capacity retention remains 80% at 1C/1C
Acidity content
≤50ppm
Applicable battery
Cylinder
Density
>1,15g/mL
Low temperature performance
Under-20℃ and for 16 hours, Capacitance play is more than 70% at 0.2C
Conductivity
10.0-12.0ms/cm
High temperature performance
Under 55℃, after 800 cycles the capacity retention is more than 80% at 1C/1C
Chroma
≤50Hazen
Advantage
This series of electrolyte is mainly suitable for the cylindrical, Soft package, Aluminum shell in which anode is NCM and cathode is composite graphite, artificial graphite.